Talc, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...Vea Mas Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. Vea Menos
Aluminum Silicate, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing f...Vea Mas Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. Vea Menos
Calcium Carbonate, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing f...Vea Mas Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm/ gauge 7+ NS. Vea Menos
Zinc Oxide, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...Vea Mas Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. Vea Menos