Alkyd Modified Acrylic Latex DTM Primer (Formulation #121813) Vanderbilt Minerals, LLC A formulation for an alkyd modified acrylic latex DTM primer which utilizes VAN GEL® SX, DARVAN® CN, BILT-PLATES® 156, and ACTIV-8®.
Alkyd Modified Acrylic Latex Maintenance Primer (Formulation #120313) Vanderbilt Minerals, LLC A formulation for an alkyd modified acrylic latex maintenance primer which utilizes VAN GEL® ES, DARVAN® 7N, and ACTIV-8®.
Aluminum Silicate, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing f...view more Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. view less
Calcium Carbonate, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing f...view more Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1. Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm/ gauge 7+ NS. view less
Dispersion-Silicate Facade Paint, Water Based (Formulation #F14402.0 [1]) Hoffmann Mineral Dispersion-Silicate Facade Paint, Water Based (Formulation #F14402.0 [1]) featuring SILLITIN N 85.
Exterior Latex Deep Toned House Paint (Formulation #040212) Vanderbilt Minerals, LLC This formulation is for an exterior latex house paint which utilizes DARVAN® CN Dispersant, VANCIDE® MZ-98 Fungicide, and BILT-PLATES® 156 Clay.
Interior/Exterior Gloss Paint (Formulation #21-10005) Patcham LTD Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...view more Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved- 7+ NS/ <10 μm. view less
Interior/Exterior Matt Paint (Formulation #21-10005) Patcham LTD Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...view more Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved. 5+ NS/ min. of 20 μm. view less
Interior/Exterior Semi Glossy Paint Waterborne Coatings (Formulation #21-10005) Patcham LTD Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...view more Gradually add Cellulosic Thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing for 10 minutes at 2 ms-1. Grind at 4 ms-1 until desired Hegman gauge is achieved. -7 NS/ min. of 15 μm. view less
Talc, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...view more Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. view less
Water Based Alkali and Efflorescence Resistant Primer based on PLIOTEC® SA 40 (Formulation #WB ARP 02) Omnova Solutions This formulation produces an alkali resistant primer. It features PLIOTEC® SA40.
Water-borne Alkyd Emulsion Red Iron Oxide Primer (Formulation #111413) Vanderbilt Minerals, LLC A formulation for a water-borne alkyd emulsion red iron oxide primer which utilizes VAN GEL® SX, DARVAN® CN, VANSIL® W-30, and ACTIV-8®.
Zinc Oxide, Extender Slurries (Formulation #21-10006) Patcham LTD Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing ...view more Gradually add cellulosic thickener in water and mix at 2.5 ms-1 for 10 minutes. Neutralize to maintain pH 8.5-9. Mix again for 10 minutes at 2.5 ms-1 . Add the raw materials in sequence. Slowly add the pigments and fillers mix thoroughly, continue mixing 10 minutes at 2 ms-1. Grind the mill base using Glass beads for 2 hours at 21 ms-1 μm / gauge 7+ NS. view less